Abstract: Sintered specimens of zirconia-10 mol% scandia pure and codoped (up to 1.25 mol%) with europium sexquioxide were prepared by solid-state synthesis, aiming to stabilize at room temperature the high-conductivity cubic phase. High-temperature X-ray diffraction and differential scanning calorimetry results reveal that small amounts of the codopant reduce the enthalpy of phase transition, and full stabilization is evidenced for 1 mol% europium sexquioxide. The low-temperature (<600 degrees C) ionic conductivity increases with increasing codopant content. (C) 2018 Elsevier B.V. All rights reserved.
Author(s): Souza, JP; Grosso, RL; Muccillo, R; Muccillo, ENS
MATERIALS LETTERS
Volume: 229 Pages: 53-56 Published: OCT 15 2018
PDF: Phase composition and ionic conductivity of zirconia stabilized with scandia and europia
DOI: 10.1016/j.matlet.2018.06.091